Room-temperature sodium-sulfur (RT Na–S) batteries have garnered increasing attention due to their high theoretical capacity and the natural abundance of sodium resources. However, they suffer from the rapid capacity decay by the chemomechanical fatigue degradation (CFD) mechanism arising from repeated solid-state volume fluctuations and partial dissolution of sulfur species that progressively weaken the percolation network, leading to irreversible structural collapse, electrical disconnection, and eventual cell failure. To address the CFD, a rigid Na3Zr2Si2PO12 interlayer (NZSP) has been introduced for simultaneous mechanical confinement and chemical polysulfide anchoring, thus limiting volume fluctuation–induced stress, preserving the percolation network, and suppressing species-driven degradation. The NZSP-modified cathode exhibits an extremely high capacity of 1035.37 mAh g−1 (0.1 A g−1, 200 cycles), along with remarkable rate capability with a capacity of 830.56 mAh g−1 at 2 A g−1 (500 cycles), 685.18 mAh g−1 at 4 A g−1 after 500 cycles, respectively. Notably, after 2,000 cycles, the NZSP-modified cathode preserves its pristine morphology and structural integrity, whereas the unmodified counterpart suffers severe CFD-induced pulverization and delamination, failing after only 659 cycles. These findings demonstrate that integrating the NZSP interlayer effectively suppresses CFD, offering a practical materials strategy for achieving long-life, high-capacity RT Na-S batteries.
Link:Interlayer design mitigates chemomechanical fatigue degradation to enable long-lived Na–S batteries - ScienceDirect